LAMAN
DOC: LAMAN-SPEC-001VERSION: 1.0EFFECTIVE: 19 OCTOBER 2026ISSUING AUTHORITY: LAMAN INTERNAL

Fabric Specification & Quality Standard

This document outlines LAMAN's internal fabric standards, detailing our material expectations, yarn specifications, and quality benchmarks across all apparel lines. It records the standards we mandate to our spinning and knitting mills, and the criteria against which incoming production lots are audited.

!

Critical Governance Boundary & Transparency Policy

This is an internal specification sheet outlining brand targets and acceptance thresholds. It is not a laboratory test report or certificate and contains no empirical test results. We refuse to publish mock laboratory stamps or fabricated PDF certificates.

Any public claims regarding fabric composition or quality must be substantiated exclusively by signed, independent third-party laboratory reports. When commercial production batches undergo official laboratory analysis, direct portal verification links and signed reports will be audited and cataloged openly in Section 5 below.

Section 01

Brand Declarations & Fiber Integrity Mandates

Raw material governance forms the cornerstone of product longevity, comfort, and brand trust. Strict enforcement of fiber composition standards ensures that every garment delivered to market meets exact physical expectations while protecting brand equity from material degradation and synthetic contamination.

Core Fiber Declarations

  • •
    Fibre Content: 100% combed cotton across every product line. Zero blends.
  • •
    Knit Structure: Single jersey (weft knit) construction for natural elasticity and airflow.
  • •
    Yarn Purity: Ring-spun combed cotton to eliminate short, bristly fibers.

Absolute Fiber Prohibitions

  • ✕
    Banned Synthetics: Polyester, nylon, elastane, and acrylic are strictly prohibited in any concentration. Synthetic blends result in immediate batch rejection.
  • ✕
    Banned Regenerated Cellulosics: Viscose, modal, and rayon are explicitly prohibited.
  • ✕
    Chemical Coatings: No synthetic silicone softening agents that degrade breathability.

Anti-Discount Commercial Policy

LAMAN operates under an explicit anti-discount pricing policy. Commercial stability depends directly on absolute material integrity.

Preventing raw material variance and eliminating synthetic substitutes directly suppresses the secondary quality downgrades—such as premature pilling, seam skewing, or severe post-wash shrinkage—that typically force apparel brands into markdown cycles.

Section 02

Fabric Line Technical Specifications

To support distinct garment silhouettes and functional fits across the product portfolio, fabric weights, yarn counts, and spinning techniques are systematically engineered. Matching precise yarn parameters to designated fabric weight classes ensures structural balance, drape consistency, and durability.

180 GSM

247 (Boxy Cut)

₹329
Nominal Weight180 GSM (±5%)
Acceptable Range171.0 – 189.0 g/m²
Fibre Composition100% combed cotton
Target Yarn Count24s Ne, combed ring-spun compact
Knit StructureSingle jersey (weft knit)
Best Suited ForExtreme 40°C summer heat, high humidity transpiration

Engineering Rationale:

Engineered for the light-to-midweight 247 silhouette. Finer 24s Ne yarn utilizing compact ring-spun technology to bind surface fibers, delivering a smooth face with minimal hairiness, fluid drape, and zero synthetic cling.
210 GSM

Relentless (Tempered Fit)

₹349
Nominal Weight210 GSM (±5%)
Acceptable Range199.5 – 220.5 g/m²
Fibre Composition100% combed cotton
Target Yarn Count20s Ne, combed ring-spun compact
Knit StructureSingle jersey (weft knit)
Best Suited ForYear-round wear, daily transitions, natural thermoregulation

Engineering Rationale:

Applied to the midweight Relentless silhouette. A 20s Ne compact yarn delivers the optimal ratio between fiber density and tensile body. Compact spinning minimizes surface pilling while retaining a tempered form without excessive rigidity.
320 GSM

Heavy (Tailored Fit)

₹549
Nominal Weight320 GSM (±5%)
Acceptable Range304.0 – 336.0 g/m²
Fibre Composition100% combed cotton
Target Yarn Count16s Ne, combed ring-spun (standard)
Knit StructureSingle jersey (weft knit)
Best Suited ForStructured drape, cool weather layering, long-term longevity

Engineering Rationale:

Designed for the Heavy silhouette. Deliberately omits the "compact" designation; the 16s Ne standard combed ring-spun spinning leaves a fuller fiber profile, producing a substantial tactile hand-feel and self-supporting drape for tailored lines.

Yarn Count & Structural Progression Matrix (LAMAN-SPEC-001 Section 3)

100% Combed Single Jersey
Technical Parameter180 GSM Line210 GSM Line320 GSM Line
Product / Fit Alignment247 (Boxy Cut)Relentless (Tempered Fit)Heavy (Tailored Fit)
Nominal Fabric Weight180 g/m²210 g/m²320 g/m²
Weight Tolerance±5% (171.0 – 189.0 g/m²)±5% (199.5 – 220.5 g/m²)±5% (304.0 – 336.0 g/m²)
Target Yarn Count24s Ne, compact20s Ne, compact16s Ne, combed ring-spun
Spinning TechniqueCompact Ring-SpunCompact Ring-SpunStandard Ring-Spun (deliberate fuller hand)
Hand-feel & BehaviorFeatherweight, breathable, high transpirationSupple, balanced density, anti-clingSubstantial, heavy architectural drape
Section 03

Physical & Chemical Laboratory Acceptance Targets

Standardized laboratory testing validates that raw fabric shipments meet defined structural, dimensional, and ecological safety thresholds prior to garment conversion. Below are the exact standards and acceptance cutoffs mandated by LAMAN to independent testing facilities.

ParameterTesting Standard / MethodAcceptance Target / Threshold
Fibre CompositionISO 1833-1 / AATCC 20A100% cotton; synthetic fibres not detected
Fabric WeightISO 3801 / ASTM D3776Within ±5% of nominal (180, 210, 320 g/m²)
Yarn CountASTM D1059 / IS 1315Within one count of target (24s / 20s / 16s Ne)
Dimensional Stability (Length)ISO 6330 (40°C, 3 washes)Not more than 3.5%
Dimensional Stability (Width)ISO 6330 (40°C, 3 washes)Not more than 3.0%
Spirality Post-WashAATCC 179 Method 1Not more than 3.0%
Bursting StrengthISO 13938-2180 GSM: >250 kPa | 210 GSM: >280 kPa | 320 GSM: >350 kPa
Pilling ResistanceISO 12945-2 (Martindale)Grade 3-4 or better (2,000 cycles)
Colourfastness to WashingISO 105-C06Grade 4 or better
Free FormaldehydeISO 14184-1Not more than 75 mg/kg
pH of Aqueous ExtractISO 30714.5 – 7.5 (Skin neutral)

Dimensional Stability & Spirality

Restricting length shrinkage to ≤ 3.5% and width shrinkage to ≤ 3.0% under ISO 6330 prevents garment distortion after consumer laundering. Spirality testing under AATCC 179 measures rotational torque; capping torque at ≤ 3.0% ensures that side seams never twist forward during wear.

Bursting Strength & Durability

Bursting strength thresholds increase proportionally with fabric weight (above 250 kPa for 180 GSM, above 280 kPa for 210 GSM, and above 350 kPa for 320 GSM under ISO 13938-2), guaranteeing high mechanical resistance under stress without seam rupture.

Chemical & Skin Neutrality

Mandating free formaldehyde levels of ≤ 75 mg/kg (ISO 14184-1) and maintaining an aqueous extract pH range of 4.5–7.5 (ISO 3071) eliminates hazardous finishing residues and ensures total skin safety in direct 40°C contact.

Section 04

Third-Party Verification & Portal Validation Protocols

Independent third-party verification provides unbiased validation of mill performance. To maintain audit integrity, this log is completed only from signed reports received directly from accredited testing facilities and verified on their portal.

Independent Verification Log (LAMAN-SPEC-001 Section 5)
Status: In Progress / Mill Sampling Phase
Fabric LineLab NameReport NumberLab Accreditation / ULRTest DateProduction BatchPortal Verified
180 GSM (247)Awaiting lab receipt———Active Batch 01Pending Lab Audit
210 GSM (Relentless)Awaiting lab receipt———Active Batch 01Pending Lab Audit
320 GSM (Heavy)Awaiting lab receipt———Active Batch 01Pending Lab Audit

Verification Directives: Records are entered only from signed test reports received directly from accredited testing facilities. Reports must be cross-verified on the issuing facility's digital portal before publication.

Direct Receipt & Portal Validation

Verification log entries may only be transcribed from official, signed test reports received directly from accredited testing facilities. Personnel must log onto the issuing laboratory's official portal to confirm report authenticity before releasing results.

Quarantine Protocol on Discrepancy

If a laboratory report cannot be validated on the issuing facility's official portal, or if data discrepancies are detected, the associated production batch is placed under immediate quarantine, blocking any fabric movement into production.

Section 05

Batch Intake & Quality Assurance Workflow

The batch intake workflow dictates the operational sequence for physical receiving, sampling, testing cross-reference, and final inventory disposition for all incoming mill shipments.

Physical Intake & Disposition Sequence

STEP 01

Incoming Mill Shipment

Receipt of knitted fabric rolls at warehouse facility.

STEP 02

Extract Batch Swatch

Quality inspectors cut test swatches directly from bulk rolls.

STEP 03

Independent Lab Audit

Dispatch swatches for ISO 1833-1 composition and mechanical audit.

STEP 04

Portal Verification

Digital authentication on testing house portal prior to sign-off.

Disposition Tri-State Decision Matrix

ACCEPT

Rendered only when verified laboratory reports confirm full compliance across all physical, chemical, dimensional, and 100% cotton fiber targets.

HOLD

Applied when test results are pending, portal verification is unconfirmed, or minor target variances require executive technical review.

REJECT

Mandated when testing reveals out-of-spec parameters or the detection of any prohibited synthetic or regenerated fibers. Lot is blocked from cutting.

Standard Batch Intake Record Checklist (LAMAN-SPEC-001 Section 6)

Batch Numbere.g. LAM-2026-B01
Supplier / MillCertified Mill Partner
Date ReceivedDD / MM / YYYY
GSM Line180 / 210 / 320 GSM
Quantitykg / pieces received
Swatch TakenYes / No
Swatch Sent to LabYes / No
DispositionAccept / Hold / Reject
Section 06

Home Verification Guide: How to Test Pure Cotton

We encourage customers and independent creators to test our garments directly. Because natural cellulose and synthetic petroleum-based fibres behave completely differently under heat, water, and static, anyone can verify fibre authenticity at home without laboratory equipment.

Fibre Identification

1. The Flame / Burn Test

🌿 Pure Cotton (LAMAN)

Burns steadily with an orange flame and a faint scent of burning paper or wood. Extinguishes cleanly and leaves a soft, crumbly grey ash that crushes to fine powder between fingertips.

✕ Synthetic Polyester

Polyester and nylon curl away from heat, melt rapidly, and produce black smoke with a pungent chemical or plastic smell. Leaves a hard, uncrushable plastic bead that clings to fabric.

Absorption & Breathability

2. The Water Droplet Test

🌿 Pure Cotton (LAMAN)

A drop of water placed on pure untreated cotton absorbs within seconds due to natural cellulose hydrophilic capillary action.

✕ Synthetic Polyester

Synthetic polyester fibres are hydrophobic (oil-based). Water droplets bead on the surface and resist immediate absorption, trapping sweat against skin.

Friction & Comfort

3. The Electrostatic Test

🌿 Pure Cotton (LAMAN)

Natural cotton fibres retain ambient moisture and exhibit neutral electrical resistance. Friction against skin produces 0 static cling or sparks.

✕ Synthetic Polyester

Polyester builds significant triboelectric electrostatic charges during movement, attracting dust and clinging uncomfortably to body hair in dry heat.

Open Testing Invitation

If you ever conduct a flame, microscopic, or chemical dissolution test on any LAMAN product and find any trace of polyester, acrylic, or synthetic fibre, email our founder directly at stores.laman@gmail.com. We will immediately refund your purchase and publish the findings publicly.

Join Owners Club →
Section 07

Sourced Science & Literature Register

Every public factual claim we publish regarding natural cotton, synthetic microfibres, and transpiration is backed by peer-reviewed literature.

Factual ClaimReference Source
Cotton absorbs, breathes and biodegrades with 0% synthetic polyester.Read Publication ↗
Polyester is a synthetic polymer derived from petrochemical crude oil refinement.Read Publication ↗
Synthetic garments shed microplastic fibres into wastewater during domestic laundering.Read Publication ↗
Pure long-staple cotton allows natural thermal transpiration in 40°C Indian climate.Read Publication ↗